Resumen
ISO 4689-3:2015 specifies a combustion/infrared method, using a high-frequency induction furnace, for the determination of the sulfur content of iron ores.
This method is applicable to sulfur contents between 0,002 % (mass fraction) and 0,25 % (mass fraction) in natural iron ores, iron ore concentrates and agglomerates, including sinter products. The method is not applicable to iron ores containing more than 1,0 % (mass fraction) of combined water. The apparatus, of which the metal filter is equipped with a heating device, can be applied to iron ores containing less than 3,0 % (mass fraction) of combined water.
Informaciones generales
-
Estado: RetiradaFecha de publicación: 2015-08Etapa: Retirada de la Norma Internacional [95.99]
-
Edición: 2Número de páginas: 13
-
Comité Técnico :ISO/TC 102/SC 2ICS :73.060.10