Тезис
This document describes two methods for measuring stress in tension under non-isothermal conditions.
— Method A: The thermal stress is measured for various pre-strain and temperature conditions as a function of time.
— Method B: The change of stress is measured in a test piece at a given strain and under variation of temperature at a given heating rate as a function of temperature. In this way, the determination of the thermal-mechanical behaviour of a rubber can be accelerated, e.g. for the purpose of comparative testing of aging or estimating the upper limit of the operating temperature.
The measurement device, which is equipped with a suitable heating chamber, is used to record the stress as a function of time or temperature until the sample breaks or the stress has approached zero or for a certain time.
Общая информация
-
Текущий статус: ОпубликованоДата публикации: 2023-01Этап: Опубликование международного стандарта [60.60]
-
Версия: 3
-
Технический комитет :ISO/TC 45/SC 2ICS :83.060
- RSS обновления
Жизненный цикл
-
Ранее
ОтозваноISO 12493:2017
-
Сейчас
-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00