Тезис
The method is based on decomposition of the test portion by 1) sintering with sodium peroxide and treatment with hydrochloric and perchloric acids and treatment with dilute nitric acid, or 2) treatment with hydrochloric, nitric and perchloric acids, evaporation, filtration of silica with any residue, fusion with sodium carbonate and dissolution in hydrochloric and perchloric acids, in both cases evaporation of the solution, filtration of the precipitated silica, ignition, and weighing, treatment of the ignited residue with hydrofluoric and sulfuric acid, ignition, and reweighing. Applies to silicon contents between 1 % and 15 % in natural iron ores, iron ore concentrates and agglomerates, including sinter products.
Общая информация
-
Текущий статус: ОпубликованоДата публикации: 1992-12Этап: Подтверждение действия международного стандарта [90.93]
-
Версия: 1
-
Технический комитет :ISO/TC 102/SC 2ICS :73.060.10
- RSS обновления
Жизненный цикл
-
Ранее
ОтозваноISO 2598:1980
-
Сейчас
ОпубликованоISO 2598-1:1992
Стандарт, который пересматривается каждые 5 лет
Этап: 90.93 (Подтверждено)-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00