ISO 14855-2:2007 specifies a method for determining the ultimate aerobic biodegradability of plastic materials under controlled composting conditions by gravimetric measurement of the amount of carbon dioxide evolved. The method is designed to yield an optimum rate of biodegradation by adjusting the humidity, aeration and temperature of the composting vessel.
The method applies to the following materials:
- natural and/or synthetic polymers and copolymers, and mixtures of these;
- plastic materials that contain additives such as plasticizers or colorants;
- water-soluble polymers;
- materials that, under the test conditions, do not inhibit the activity of micro-organisms present in the inoculum.
Общая информация
-
Текущий статус: ОтозваноДата публикации: 2007-08Этап: Отмена международного стандарта [95.99]
-
Версия: 1
-
Технический комитет :ISO/TC 61/SC 14ICS :83.080.01
- RSS обновления
Жизненный цикл
-
Сейчас
-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
Исправления
Исправление текущего издания; предоставляются бесплатно; не включены в текст действующего стандарта.ОтозваноISO 14855-2:2007/Cor 1:2009
-
00
-
Пересмотрен
ОпубликованоISO 14855-2:2018