Тезис
Two methods for the measurement are specified: Method A (Ball displacement method): Determination of the viscosity of a pitch at a given temperature determined using a sample of pitch having similar characteristics by measurement of the time a ball, drawn by a defined force, requires to traverse a fixed distance within a measuring tube filled with the sample of molten pitch. Method B (Rotation of a cylindrical body method): Measurement of the shear stress of a substance at a selected rotational speed at a given temperature by means of a system composed of a cylindrical-conical body revolving in the substance contained in a cylindrical vessel.
Общая информация
-
Текущий статус: ОпубликованоДата публикации: 1985-06Этап: Подтверждение действия международного стандарта [90.93]
-
Версия: 1
-
Технический комитет :ISO/TC 226ICS :71.100.10
- RSS обновления
Жизненный цикл
-
Сейчас
ОпубликованоISO 8003:1985
Стандарт, который пересматривается каждые 5 лет
Этап: 90.93 (Подтверждено)-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00